Aging Chemical - Bronzing Solution - Metal Aging - CC60
 
 
How to make up:
 
  • 1 part CC60 to 4 parts water (by volume)
  • At temperature 18 to 60 celsius
  • Time 30 seconds to 2 minutes
  • Colour: for darker shades use 1 to 3 parts for medium shades are produced in 30 seconds
  • For best results parts should be clean when immersed in this solution
  • A tank with polythene, pvc or rubber lined steel is ideal
  • A heater is not required but an extraction is necessary
  • To be used on copper or brass
  • Gives a bronze/brown finish